| Condition | Optimum | Operating Range | Units | Notes | ||
|---|---|---|---|---|---|---|
| Injection | Cooling | Discharge | ||||
| (Temperature) | 120 | 60 | 60 | 50 - 190 | °C | N/A |
| Pressure | 1500 | Ambient | 240 | 0 - 2000 | psi | N/A |
Management Practices
Known Faults
Improper cooling can lead to polymer sticking to the mold. As the mold cools, the polymer should shrink and this shrinkage helps it to dislodge from the mold surface.